Наукові статті

Permanent URI for this collectionhttps://repository.lntu.edu.ua/handle/123456789/329

Browse

Search Results

Now showing 1 - 10 of 37
  • Item type:scientificarticle.listelement.badge,
    In-situ ceramic formation in a (NbC–TiC–TiB2) precursor-modified Inconel 718 via SPS and laser surface melting: Composite structure evolution and tribological performance
    (2026-10) Chabak, Yuliia; Efremenko, Vasily; Zaichuk, Nataliia; Puchý, Viktor; Efremenko, Bogdan; Petrišinec, Ivan; Kamyshnykova, Kateryna; Sili, Ivan
    An Inconel 718-based composite reinforced with a multicomponent NbC-TiC-TiB2 ceramic precursor (5-20 vol%) was fabricated via a dual-stage processing route combining spark plasma sintering and subsequent laser surface melting in air. This study investigated the structural and mechanical evolution of the composite through the in-situ alteration of the ceramic phase constitution. Under superheated molten pool conditions, complete dissolution of the precursor occurred, driving a non-equilibrium crystallization pathway. During primary crystallization, complex Ti-Al-O cores formed, followed by heterogeneous nucleation of multicomponent ceramic phases comprising faceted (Nb,Ti,Cr,Mo) (B,C) carboboride shells and a discontinuous interdendritic eutectic network of (Cr,Nb,Mo,Ti)B2 borides. Progressive precursor addition increased the area fractions of equiaxed ceramic particles and eutectic boride inclusions to 3.3% and 18.0%, respectively, while promoting non-linear phase coarsening due to the expanded solidification window. This structural modification increased nanoindentation hardness by 36% (from 3.22 to 4.38 GPa) and modulus by 14% (from 200.4 to 228.7 GPa), while maintaining the indentation plasticity parameter at a comparable level. Tribological testing showed that increasing the precursor content drove a progressive reduction in friction coefficient from 0.95 to 0.77 and a 2.4-fold decrease in wear rate. SEM and EDS examinations of the wear tracks indicated a transition from severe adhesive and oxidative wear toward the formation of compact tribolayers and reduced material removal in the precursor-modified composites. These results demonstrate that the NbC-TiC-TiB2 precursor substantially influences phase evolution during laser processing and improves the wear resistance of the resulting composite layers.
  • Item type:scientificarticle.listelement.badge,
    Technologies and models for effective cleaning of rolling bearings from various types of operational contamination
    (United Kingdom, 2026) Kostyunik, Ruslan; Mikosianchyk, Oksana; Stelmakh Alexandr; Kushchev Aleksei; Fedosov, Serhii; Shymchuk, Serhii; Zaichuk, Nataliia; Shymchuk, Oleksandr
    Ensuring the necessary cleanliness of rolling bearings is a very complex and important scientific, industrial, and economic problem. Solving this problem allows for increasing the accuracy of machines and equipment that contain rolling bearings, significantly improving their operational properties and durability. As a result, this approach leads to a reduction in the use of metal, lubricants, and energy resources, as well as noise and vibration [1–3]. Ensuring technological cleanliness is relevant for both new bearings and those that have been in service and are being reused. The main types of contamination are metal particles (microchips formed during cutting or wear products), corrosion products, lubricant polymerization products, or accidental contamination from the external environment. Therefore, to solve the problem of ensuring the necessary cleanliness of ball bearings of various sizes, we have developed a model and technology for cleaning such bearings from various types of technological contamination, which is described in detail in this scientific work.
  • Item type:scientificarticle.listelement.badge,
    Impact of acidic environments on timber density
    (2026-02-13) Vereshko, Oleh; Homon, Sviatoslav; Melnyk, Yuliia; Gomon, Svyatoslav; Boyarska, Inna; Gomon, Petro; Chapiuk, Oleksandr; Andrii, Pavluk
    A series of experimental studies have been conducted with the objective of determining the density of birch and pine wood as a function of the period of impregnation with acetic, lactic and hydrochloric acids. The results of a new experimental study on the effect of acidic media on the density of pine and birch wood, with samples exposed for different periods prior to analysis, have been obtained. It has been demonstrated that the density of timber undergoing impregnation with a range of acids exhibits a consistent increase. However, a notable elevation is observed exclusively during the initial 28-day period, with a range of 41.3% to 86.0%. Over the subsequent five-month period, the density of the samples exhibited an increase of only 1.5% to 7.8%.
  • Item type:scientificarticle.listelement.badge,
    In-situ carboboride-reinforced metal matrix composites via spark plasma sinterning-laser surface melting hybrid processing: Microstructure and wear behavior
    (2026) Zaichuk, Nataliia; Efremenko, Vasily; Chabak, Yuliia; Petrišinec, Ivan; Efremenko, Bogdan; Кovbasiuk, Taras; Sili, Ivan; Puchý, Viktor; Lekatou, Angeliki
    This study compares the microstructure, hardness, and dry-sliding wear behavior of a new multicomponent Fe–C–B–W–Mo–V–Cr–Ti carboboride/metal (martensite) matrix composite fabricated via spark plasma sintering (SPS) and laser surface melting (LSM), against its sand-cast reference – multicomponent cast iron (MCCI). The SPS/LSM specimens exhibited a 1 mm thick, porosity-free surface layer with a hierarchical composite microstructure. This layer consists of hard eutectic colonies (“Chinese script” (CS) and ledeburite) and equiaxed (Ti,W)-rich multiphase carboboride/C– O –N inclusions within a martensitic matrix. Internally, the CS colonies consist of interconnected (W,Mo,Cr,V)2(B,C)5 eutectic plates branching within the local martensitic matrix, whereas the ledeburite colonies consist of a matrix of (Fe,Cr,W,Mo,V)3(C,B) plates penetrated by fine martensitic rods. Although similar to MCCI in morphology and phase composition, the SPS/LSM structure was notably refined. Heat treatment (HT) of the SPS/LSM specimens (annealing at 1150 °C for 2 h followed by oil quenching) increased matrix carbon, retained austenite volume fraction and dislocation density, and induced alloying element redistribution between microconstituents. The SPS/LSM composite outperformed MCCI in dry-sliding wear resistance (1.7 times as-fabricated, 1.5 times post-heat treated). Laser melting and post-heat treatment increased the wear resistance of the SPS alloy by a factor of 3.2. The SPS/LSM and SPS/LSM/HT composites wore through low-cycle fatigue, with limited microcracking and delamination, abrasion and surface oxidation. In contrast, MCCI exhibited severe surface deterioration characterized by extensive plastic flow and lateral build-up formation, which preceded material removal. © 2026 The Authors.
  • Item type:scientificarticle.listelement.badge,
    Розробка біокомпозитних матеріалів на основі глютину а волокон льону
    (Луцьк: ЛНТУ, 2026) Садова, Оксана Леонідівна
    В статті приведено дослідження міцності на стискання біокомпозитних матеріалів на основі водного розчину глютину та подрібнених волокон технічного льону довжиною 5 мм. Розроблено біокомпозитні матеріали з різним співвідношенням компонентів: 50% розчину глютину та 50% волокон льону; 46% розчину глютину та 54% волокон льону; 43% розчину глютину та 57% волокон льону; 40% розчину глютину та 60% волокон льону. Руйнування біокомпозитних матеріалів з різним співвідношенням компонентів за нижчих ступенів підсушування композиції (5-15%) під дією стискаючого навантаження супроводжується пластичною деформацію з утворенням зсувних тріщин. Максимальні значення міцності на стискання 71,7 МПа отримано для біокомпозитних матеріалів з вмістом 43% розчину глютину та 57% подрібнених волокон льону за ступеня підсушування композиції 20%. Подальше збільшення вмісту наповнювача або надмірне підсушування композиції погіршує змочуваність волокон в'яжучим, що призводить до крихкого руйнування та розколювання матеріалу.
  • Item type:scientificarticle.listelement.badge,
    Composites Based on PLA/PHBV Blends with Nanocrystalline Cellulose NCC: Mechanical and Thermal Investigation
    (2024-12-10) Bazan, Patrycja; Rochman, Arif; Mroczka, Krzysztof; Badura, Kamil; Melnychuk, Mykola; Nosal, Przemysław; Węglowska, Aleksandra
    This study investigates the physical and mechanical properties of biodegradable composites based on PLA/PHBV blends modified with different content of nanocrystalline cellulose (NCC) of 5, 10, and 15 wt.%. Density measurements reveal that the density of the composite increases with increasing NCC content. Water absorption tests demonstrate a gradual increase in the composite water content with increasing incubation time, reaching stabilization after approximately 30 days. Mechanical testing was also carried out on both on conditioned samples after the process of hydrolytic degradation and accelerated thermal aging. The conditioned composites show an increase in the stiffness of the materials with increasing content of nanocrystalline cellulose. The ability to deform and the ability to absorb energy when the sample is dynamically loaded decrease. The repeated strength tests, after the process of incubation of samples in water and after the process of accelerated thermal aging, show the degradation of composite materials; however, it is noticed that the introduction of cellulose addition reduces the impact of the applied artificial environment in aging tests. The findings of this study indicate promising applications for these types of materials, characterized by high strength and biodegradability under appropriate conditions. Household items such as various containers or reusable packaging represent potential applications of these composites.
  • Item type:scientificarticle.listelement.badge,
    Vibration Welding of PLA/PHBV Blend Composites with Nanocrystalline Cellulose
    (2024-12-15) Bazan, Patrycja; Kozub, Barbara; Rochman, Arif; Melnychuk, Mykola; Majewska, Paulina; Mroczka, Krzysztof
    Thermoplastic composites have garnered significant attention in various industries due to their exceptional properties, such as recyclability and ease of molding. In particular, biocomposites, which combine biopolymers with natural fibers, represent a promising alternative to petroleum-based materials, offering biodegradability and reduced environmental impact. However, there is limited knowledge regarding the efficacy of joining PLA/PHBV-based biocomposites modified with nanocrystalline cellulose (NCC) using vibration welding, which restricts their potential applications. This study demonstrates that vibration welding enables efficient bonding of PLA/PHBV composites with NCC, resulting in strong, biodegradable, and environmentally friendly materials. The investigation revealed that the addition of nanocrystalline cellulose (NCC) at 5, 10, and 15 wt.% significantly enhanced the strength of welded joints, with the highest strength achieved at 15% NCC content. Microstructural analysis using scanning electron microscopy (SEM) and deformation studies with digital image correlation (DIC) indicated that a higher NCC content led to greater local deformation, reducing the risk of brittle fracture. Mechanical hysteresis tests confirmed the composites’ favorable resistance to variable loads, highlighting their stability and energy dissipation capabilities. Optimization of welding parameters, such as vibration amplitude, welding time, and pressure, is crucial for achieving optimal mechanical performance. These findings suggest that PLA/PHBV composites modified with NCC can be utilized as durable and eco-friendly materials in various industries, including automotive and packaging. This research presents new opportunities for the development of biodegradable high-strength materials that can serve as alternatives to traditional plastics.
  • Item type:scientificarticle.listelement.badge,
    Properties of Perlite-Based Geopolymer as a Thermal Insulation Material for Building Efficiency
    (2025) Polivoda, Nina; Melnychuk, Mykola; Kozub, Barbara; Ostapchuk, Roman; Babych, Yaroslaw
    Globally, the key issues related to technology and materials are the reasonable consumption of exhaustible resources, increasing technological efficiency, reducing waste, and sustainable production. The construction industry is responsible for huge carbon dioxide emissions and other harmful waste in this context. Moreover, it requires about 16 percent of the world’s annual energy use for the production of cement-based products. Experts estimate that without effective changes, the negative impact on the environment and consumption will increase to 25% by 2050. This paper presents a geopolymer based on expanded perlite up to 85% that can be used as a modern lightweight thermal-insulation construction material. The results showed that the density of the samples varied from 330 kg/m3 to 510 kg/m3, the bending strength was from 1 MPa to 2 MPa, the compressive strength was from 13.5 MPa to 21 MPa, the thermal conductivity was from 0.09 W/m K to 0.130 W/m K, the water absorption coefficient was from 77% to 137%, and the total porosity of the material was from 60% to 65%. The results meet the requirements for lightweight building materials for wall construction regarding the leading indicators. Still, high water absorption significantly decreases strength and thermal conductivity after 100 h of the aging process. To reduce the water absorption of the perlite-based geopolymer, research is planned to apply a hydrophobic coating based on metakaolin.
  • Item type:scientificarticle.listelement.badge,
    Thermo-Mechanical Properties of Perlite Composite
    (2021) Melnychuk, Mykola; Poteichuk, Mykhailo; Kashytskyi, Vitalii; Sosnowski, Marcin; Kutsyk, Serhii
    Currently, perlite is used in the insulation of facades, roofs, ceilings, based on perlite, heat-insulating plasters, masonry mortars, and even adhesive compositions are produced. However, practically not used as a monolithic-structural material. Expanding the production of heat-insulating perlite materials for various purposes will inevitably be allowed to reduce heat loss and the high cost of fuel. Perlite materials can improve the physical properties of existing structures. A significant advantage of the use of perlite as a heater is a reduction in a fire hazard and an increase in the fire resistance of building structures. The article presents the results of a study of the monolithic heat-insulating material based on expanded perlite of deposit “Fogosh” (Zakarpatskyi region, Ukraine) and liquid silicate sodium glass. The basic thermal, mechanical properties, and structures of this material and compliance with the standard are investigated. In this article, describe a complex of properties of new thermal insulation material that has: ρ = 219 kg/m³, λ = 0.087 W/(m K), σc = 9.1 MPa. It is established that the investigated perlite composite according to its strength and thermal conductivity characteristics can be recommended as thermal insulation and structural material for thermal power equipment isolation.
  • Item type:scientificarticle.listelement.badge,
    The Influence of the Addition of Basalt Powder on the Properties of Foamed Geopolymers
    (MDPI AG, 2024-05-14) Łach, Michał; Kozub, Barbara; Bednarz, Sebastian; Bąk, Agnieszka; Melnychuk, Mykola; Masłoń, Adam
    Geopolymers are binder materials that are produced by a chemical reaction between silica or aluminum compounds with an alkaline activating solution. Foamed geopolymer materials are increasingly being cited as a viable alternative to popular organic insulation materials. Since the foaming process of geopolymers is difficult to control, and any achievements in improving the performance of such materials are extremely beneficial, this paper presents the effect of the addition of basalt powder on the properties of foamed geopolymers. This paper presents the results of physicochemical studies of fly ash and basalt, as well as mechanical properties, thermal properties, and structure analysis of the finished foams. The scope of the tests included density tests, compressive strength tests, tests of the thermal conductivity coefficient using a plating apparatus, as well as microstructure tests through observations using light and scanning microscopy. Ground basalt was introduced in amounts ranging from 0 to 20% by mass. It was observed that the addition of basalt powder contributes to a reduction in and spheroidization of pores, which directly affect the density and pore morphology of the materials tested. The highest density of 357.3 kg/m3 was characterized by samples with a 5 wt.% basalt powder addition. Their density was 14% higher than the reference sample without basalt powder addition. Samples with 20 wt.% basalt addition had the lowest density, and the density averaged 307.4 kg/m3. Additionally, for the sample containing 5 wt.% basalt powder, the compressive strength exceeded 1.4 MPa, and the thermal conductivity coefficient was 0.1108 W/m × K. The effect of basalt powder in geopolymer foams can vary depending on many factors, such as its chemical composition, grain size, content, and physical properties. The addition of basalt above 10% causes a decrease in the significant properties of the geopolymer.